MEMSnet Home: MEMS-Talk: Is there any way I can deposit gold onto pyrex wafer directly?
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-22
sokwon Paik
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-23
Gautham V
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-23
transene
Is there any way I can deposit gold onto pyrex wafer directly?
sokwon Paik
2003-04-22
I'm a student of Texas A&M University.
As far as I know, gold doesn't attach to pyrex glass
directly. But I think if I use sputtering machine then
it might be possible.
Anybody tried to attach gold directly onto pyrex
wafer?
One more question. Is there platinum sputtering source
exist?
If so, how much is it? Please answer me the question.
I appreciate your any reply.
Thanks,

sokwon Paik


__________________________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo
http://search.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing