Dear Kris,

We use Shipley S1813 and it works fine. Our cyanide-based plating
solution is Technic Orotemp 24RC. They intend it for use with photoresist
patterned substrates. If you are having trouble you might try that bath.

Jordan

> ------------------------------
>
> Message: 6
> Date: Wed, 23 Apr 2003 23:02:35 -0700 (PDT)
> From: krishna 
> Subject: [mems-talk] Photoresist
> To: General MEMS discussion 
> Message-ID: <[email protected]>
> Content-Type: text/plain; charset=us-ascii
>
> I am looking for a supplier who can supply positive
> photoresist that is suitable for gold electroplating.
>
> The plating bath i am using is of cyanide type and i
> am looking for the photoresist that can resist cyanide
> attack.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation