MEMSnet Home: MEMS-Talk: electro and electroless plating for Ni?
electro and electroless plating for Ni?
2003-05-05
Chen Yan
2003-05-07
Absara Micro Systems
2003-05-09
Dr. Hermann Oppermann
2003-05-06
[email protected]
2003-05-06
Christopher Blanford
2003-05-21
Chen Yan
2003-05-27
Absara Micro Systems
electro and electroless plating for Ni?
Dr. Hermann Oppermann
2003-05-09
Hi,

you can download informations about electroless Ni bumping from the web
site
http://web.pb.izm.fhg.de/avt/050_download/index.html

Hermann Oppermann



Chen Yan wrote:

>Hi there,
>
>Any infomation about electro and electroless plating for Ni?
>
>Thank you for any help!
>
>chenyan
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>
>

--

Dr. Hermann Oppermann
Fraunhofer IZM
Gustav-Meyer-Allee 25
D-13355 Berlin, Germany
--------------------------------------------------
phone: +49-30-46403-163, -160
Fax:   +49-30-46403-161
email: [email protected]
--------------------------------------------------
Dept. Chip Interconnection Technologies
Group Optoelectronics, HF and Sensor Integration
http://www.izm.fhg.de/avt/opperm.htm
--------------------------------------------------





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing