vikas vadloori
cu etching
vikas vadloori
2003-05-19
hello
we are trying to etch Cu of thickness 20-25 micron
plated on silicon.we are trying with  HNO3 solution
but under cut occuring
 sugession for improving etching & good side wall
definition required
thankyou in advance for your help
best regards
vikas

__________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
http://search.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing