Houri Johari
2003-06-09
Dear Rajkumar
I used polyimide as a sensitive layer in humidity sensor.
Sincerely
Houri Johari

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Raj Kumar
Sent: Saturday, June 07, 2003 2:56 AM
To: [email protected]
Subject: [mems-talk] Polymer for Humidity (Rh) sensor


Hello MEMSnet friends
      Can any body tell me the detail of the supliers of humidity
sensitive polymers that can be used for making Rh sensors.

Sincerely yours

   Rajkumar
SCL, India
________________________________________________________________________
_____





_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing