MEMSnet Home: MEMS-Talk: RE: Cu Metal Etchant (Luciano Scaltrito)
RE: Cu Metal Etchant (Luciano Scaltrito)
2003-07-04
luciano scaltrito
RE: Cu Metal Etchant (Luciano Scaltrito)
luciano scaltrito
2003-07-04
Ferric Chloride used to make printed circuit boards is a good etchant.
you have to use a buffer layer like Ta/Au or Ti/Au.


--------------------------------------------------------------------------------
--------
                 ~ The truth is out there ~
Ing. Luciano Scaltrito
Dipartimento di Fisica
Politecnico di Torino
C.so Duca degli Abruzzi, 24
10129 Torino, Italy
tel +39 011 564.7305/564.4160
fax +39 011 564.7399
E-mail : [email protected]
http://www.polito.it/centri/laborato/limadel/film/index.html
--------------------------------------------------------------------------------
--------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group
Harrick Plasma, Inc.