Dear collegues:
We would like to inquire if any of you have tried to dilute BCB (Cyclotene)
available from Dow Chemicals to achieve thinner coatings. Please, advise on
the procedure.
Thank you very much.

Ivan Shubin
Research Scientist
ECE Department, EBU-1, M.C. 0407
University of California, San Diego
La Jolla, CA 92093
ph./fax (858) 534-6570


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group
Harrick Plasma, Inc.