Si sputtering maximum thickness
2003-08-26
GuyHaché
Si sputtering maximum thickness
GuyHaché
2003-08-26
Hi,

I would like to know what is the range of the typical maximum thickness that I
could achieve sputtering Si?

Also, the rate of deposition would vary between what?

Thank's,

Guy Haché, M.Sc.A.
Assistant de recherche, research assistant
--------------------------------------------------------
Département de génie électrique et de génie informatique
Université de Sherbrooke
2500, boulevard Université
Sherbrooke (Québec) Canada
J1K 2R1
Téléphone/phone : (819) 821-8000 3706
Télécopieur/fax : (819) 821-7937
e-mail: [email protected]
--------------------------------------------------------




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Harrick Plasma, Inc.
MEMStaff Inc.