how to attach antibodies on gold
Bill Moffat
2003-09-02
A normal adhesion promoter for gold is a mercapto silane. A number of companies
are using a silylation unit to put marcapto silanes down on Bio-Chips for DNA
adhesion.  Contact me directly for further information.  Bill Moffat

-----Original Message-----
From: harshal rokade [mailto:[email protected]]
Sent: Friday, August 29, 2003 11:27 PM
To: [email protected]
Subject: [mems-talk] how to attach antibodies on gold


hi alll,
how to attach antibodies on gold which is acting as a piezo material on oxide
cantilever??
thanks in advance.


-Regards

Harshal Rokade

---------------------------------
Do you Yahoo!?
Yahoo! SiteBuilder - Free, easy-to-use web site design software
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Mentor Graphics Corporation
MEMS Technology Review