Ni diffusion on Au under 800C
[email protected]
2003-09-06
I'm now working for a MEMS devices which work under 600 C. 2 microns
electroless Ni and 2 microns Au are plated on Cu substrate. Some white
spots is observed after 600 C thermal testing. I guess that would be due to
metal diffusion. Would profession suggest a better diffusion barrier rather
than Ni?

Benny Hong



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review