Hello all,
  i am interested in developing Al-pyrex anodic bonding.  I have performed
several experiments using thin film aluminum and pyrex glass and have been only
successful a few times.  i have not been able to make my process highly
repeatable. I would appreciate advice from anyone who has had experience with
this process.

Regards.
Ryan

Ryan D. Pooran
Ph.D Candidate Microelectronics-Photonics
Mechanical Engineering Department
University of Arkansas
Fayetteville, AR 72701
Ph:479-575-4150
Fax: 479-575-6982
e-mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing