MEMSnet Home: MEMS-Talk: BCB as pretectd layer
BCB as pretectd layer
2003-09-21
Mohamed Saadoui
2003-09-22
Shay Kaplan
2003-09-22
Balaji Lakshminarayanan
BCB as pretectd layer
Mohamed Saadoui
2003-09-21
Hi,


I want to use CYCLOTENE resine BCB-4000 as protective coating during silicon
etching in pottasium hydroxide KOH at 85C, which must be removed at the end of
processing.

It will be very helpful if anyone can give information about this BCB process.

Thanks and Regards,

Mohamed SAADAOUI
Laboratoire d' Analyse
et d' Architectures Systemes
LAAS- TOULOUSE. france




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics