A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Very thick silicon wafers
Very thick silicon wafers
2003-10-01
lucia beccai
2003-10-01
Kenneth Smith
2003-10-01
Kim Norris
2003-10-01
John Fuste
2003-10-02
[email protected]
Very thick silicon wafers
John Fuste
2003-10-01
hello Lucia,

you can try a company named Okmetic-they produce various types of silicon
wafers. their website is as follows:www.okmetic.com/  Good luck

Lenny Fuste
Production Engineer
Veeco Probes



-----Original Message-----
From: lucia beccai [mailto:[email protected]]
Sent: Wednesday, October 01, 2003 7:23 AM
To: [email protected]
Subject: [mems-talk] Very thick silicon wafers



Hi,

does anyone know about silicon companies who can supply 4" and 5"
silicon wafers having a thickness of 4 -5 mm ?
Thanks in advance for your information.

Lucia
----------------------------------------------
Lucia Beccai, Ph.D.
Research assistant
CRIM Lab - Polo Sant'Anna Valdera - Scuola Superiore Sant'Anna
Viale R. Piaggio 34 - 56025 Pontedera (Pisa) - Italy
phone: +39 050 883 488
fax  +39 050 883 496/497
http://www-crim.sssup.it/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
MEMS Technology Review
MEMStaff Inc.