Solgel process / low temperature bonding
2003-10-23
Robert Smith
2003-10-31
BRAD JOHNSON
2003-11-03
Mark M Crain
Solgel process / low temperature bonding
Mark M Crain
2003-11-03
HI Brad,

Could you go into more detail about your bonding process and the bonding
material?

Thanks,

Mark Crain
University of Louisville
502/852-1572

>>> [email protected] 10/31/03 1:26 PM >>>
Hello Bob,
How low a temp are you looking at?  We have achieved very good results
bonding Pyrex to Pyrex and Pyrex to Silicon at room temp then annealing
at much less then 300C.  If you are looking for a permeant bond this
would work great.

Brad

Brad Johnson
Suss MicroTec
Applications Engineer
1-480-557-9370 Ext119
1-800-685-7877 Ext119
[email protected]


>>> [email protected] 10/23/03 06:44PM >>>
Hello All,

Is sol-gel process a good method to bond glass?  If anybody has
experience with that type of procedure, can you please share it with me?

Are there any other way of bonding glass using low temperature?

Any information will be appreciated.

Thanks,

Robert


---------------------------------
Do you Yahoo!?
The New Yahoo! Shopping - with improved product searchFrom
[email protected] Thu Oct 23 20:00:18 2003
Received: from mb1i1.ns.pitt.edu ([136.142.185.161])
        by kronos.mems-exchange.org with esmtp (Exim 4.22)
        id 1ACpNJ-0003VC-MI
        for [email protected]; Thu, 23 Oct 2003 20:00:17 -0400
Received: from CONVERSION-DAEMON by pitt.edu (PMDF V5.2-32 #41462)
 id <[email protected]> for [email protected];
Thu,
 23 Oct 2003 19:59:55 EDT
Received: from [10.0.38.254] ([68.166.44.119])
 by pitt.edu (PMDF V5.2-32 #41462) with ESMTPA id
 <[email protected]> for [email protected]; Thu,
 23 Oct 2003 19:59:54 -0400 (EDT)
Date: Thu, 23 Oct 2003 19:59:53 -0400
From: Alik Widge 
Subject: Re: [mems-talk] Photosensitive SAM
In-reply-to: <005e01c398fe$c30cffb0$dc87dc80@YiPing>
Originator-info: login-id=alik; server=postoffice.srv.cs.cmu.edu
To: General MEMS discussion 
Message-id: <86180711.1066939193@[10.0.38.254]>
MIME-version: 1.0
X-Mailer: Mulberry/2.2.1 (Win32)
Content-type: text/plain; charset=us-ascii; format=flowed
Content-disposition: inline
Content-transfer-encoding: 7bit
References: <005e01c398fe$c30cffb0$dc87dc80@YiPing>
X-Spam-Status: OK 0.000
X-Vetted: message OK
X-Mailman-Approved-At: Fri, 24 Oct 2003 10:40:10 -0400
X-BeenThere: [email protected]
X-Mailman-Version: 2.1.1
Precedence: list
Reply-To: General MEMS discussion 
List-Id: General MEMS discussion 
List-Unsubscribe:
,
        
List-Archive: 
List-Post: 
List-Help: 
List-Subscribe:
,
        

Yi-Ping,

Most self-assembled monolayers are sensitive to UV-induced desorption if

the dose is high and long enough, especially the thiol-based SAMs. Look
through George Whitesides' paper archive at Harvard and you'll find 99%
of
what you need.

Alik


--On Thursday, October 23, 2003 8:44 AM +0800 Yi-Ping Ho 
wrote:

> Hi there,
>
> Is there any one who knows how to make the photosensitive SAM(Self
> Assemble Monolayer)? Or any reference papers?
>




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation