A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: deep trenches in SU-8
deep trenches in SU-8
2003-11-05
Olga Makarova (2 parts)
2003-11-06
franCk
deep trenches in SU-8
Olga Makarova
2003-11-05
Hello all,
I have a problem in cleaning out 1mm deep and 40um wide trenches in
continuos SU-8 layer.  Trenches that are close to the edges are clean,
while the others contain the residue that I can not remove.  I do
developing in SU-8 developer with magnetic stirring.  The use of
ultrasound damages the structure.  Does anybody know how to improve my
developing process?

Thank you very much,

Olga


makarova.vcf (text/x-vcard, 363 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.