how can i oxidate the vertical cliff
2003-11-08
zhgf
2003-11-10
[email protected]
how can i oxidate the vertical cliff
[email protected]
2003-11-10
You could deposit a thin layer of silicon nitride before you ICP etch through
the wafer. This will protect the surface top and bottom of the wafer from
oxidizing during thermal processing then you can plasma etch removal of nitride
as the final step. Bob Henderson