At 12:01 PM 11/12/2003, you wrote:

>I need to send out 100 mm wafers for either a rapid thermal anneal @ 1100 C in
>N2 for 10 minutes, or a longer anneal @ 800 C.   I have been having trouble
>finding a vendor whose equipment is running, and who will accept the wafers
>after they have been exposed to metal.  Does anybody know of any commercial
>services out there ?
>
>Michael
Try www.processpecialties.com 800-533-8820


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics