We are interested in testing and ordering a complete, turnkey Ion Assisted
Deposition evaporator. We would rather not purchase the ion source and
evaporator separately, which seems to be the standard operating procedure.
This would be a machine for R&D, so we are not interested in paying for lots
of bells & whistles, or in buying more than one (at this time).

In addition, we would consider sending wafers out of house for IAD. We are
most concerned with film stress and dielectric constant; these are not
optical coatings, and so the parameters would need to be optimized differently.


 Please forward any relevant information to: [email protected].

Many thanks!

Susan Eshelman
Susan Eshelman
Member, Technical Staff
Raytheon TI Systems
[email protected]
(972) 995-2476


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.
MEMS Technology Review