Hello, Friends,

I am planning to deposit/sputter 1um-thick tungsten onto the BCB substrate. is
there anyone who has such kind of experience so can give me some advice? I am
concerned with the adhesion and thickness limit and the uniformity regarding
this process.

Thanks

Michael