Tapering SU-8 in z-axis
2004-04-29
Michael L
2004-04-29
Brubaker Chad
Tapering SU-8 in z-axis
Brubaker Chad
2004-04-29
Michael,

The primary method I have seen for tapering SU-8 is through the use of a gray
scale mask.   Basically, this is a mask where, instead of just having regions of
full transparency or full reflection (i.e., glass and chrome), you have areas
with variable transpanrancy.

My understanding is that, with SU-8, this may need to be performed on a glass
substrate through the backside of the wafer, since SU-8 is negative tone, and
exposing from the top may create a reversed profile.

Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.

 -----Original Message-----
From:   [email protected] [mailto:mems-talk-
[email protected]]  On Behalf Of Michael L
Sent:   Thursday, April 29, 2004 5:07 AM
To:     [email protected]
Subject:        [mems-talk] Tapering SU-8 in z-axis

Hello,

Does anyone know of a simple method for vertically tapering SU-8? I have
heard of people who have achieved this, but haven't seen anything mentioned
in the literature.

Regards,

Michael

_________________________________________________________________
It's fast, it's easy and it's free. Get MSN Messenger today!
http://www.msn.co.uk/messenger


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer