Hi, all
Tungsten was sputtered on silicon substrate and went through rapid thermal
anneal for 1-5s at 900C. I would expect around 30 nm tungsten silicide formed
and would like to measure it. does anyone know selective etch between tungsten
and tungsten silicide ? Thanks
--
Jialin Zhao
204 Cushing Hall
Department of Electrical Engineering
University of Notre Dame
Notre Dame, IN 46556
Tel: 574-6319011








reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.