MEMSnet Home: MEMS-Talk: Selective Etch - oxide/bpsg
Selective Etch - oxide/bpsg
2004-05-10
Avi Laker
2004-05-10
vijay j
Selective Etch - oxide/bpsg
vijay j
2004-05-10
hello,
       HF wiil be solution for your problem

byeee

Avi Laker  wrote:

Anyone have or recall an etchant that can selectively etch thermal oxide faster
then softer glasses such as BPSG? I recall using one may years ago wrt to a
reflow
process.

al

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
Yahoo! India Matrimony: Find your partner online.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing