I don't know about e-beam resists, but with UV resist you can do a UV cure -
1 hour under 248 nm light with a high temperature bake - which crosslinks
the resist and makes it insoluble.  Shipley should have a white paper on the
process.  Getting the resist off afterwards can be a trick, we've used a
very long O2 plasma.  Our resist was thicker than you are using - between
..75 and 1.5 microns.  I forget the number, but it was one of shipey's
standard UV resists.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of olivier boulle
Sent: Saturday, July 03, 2004 10:23 AM
To: [email protected]
Subject: [mems-talk] resist resistant to solvent


Dear Colleagues,
I am looking for a thin resist (300nm), resistant to acetone and
trichloroethylene, that can be easily etched with O2 plasma.
I plan to use it in a bilayer configuration PMMA/resist. I will transfer
patterns defined by e-beam lithography by etching the resist with O2
plasma. All the process must be made at low temperature (T<140°C). I
already tried Su 8, but it was too rough after O2 plasma for my process.
Does anyone ever heard about such a resist?
I would be very pleased for any suggestion,
Thanks a lot,
Olivier Boulle
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics