Hello,

I have sticking problems of my evaporated copper on evaporated titanium. Does
someone had the same problem? solutions? Is it because of the titanium oxide?
How can I remove it if so? Is the adhésion of copper on chromium better?

Best regards,

Patrick Poissant

___________________________________________________
   M.A.Sc. Student
   Dept. of Electrical Engineering
   Université de Sherbrooke
   Sherbrooke (Québec) J1K  2R1
   CANADA
   [email protected]
   Sherbrooke Microelectronics Research Group
   www.gel.usherb.ca/gms

   Anyone who has never made a mistake has never tried anything new - Albert
Einstein


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing