Eric,

I've used a bake process for 20µm thick AZ9260 that involves the following:

Moderately increased temperature
Moderately extended bake time
Specific ambient conditions (unfortunately, I cannot disclose in a public forum,
as it is proprietary)
Ramped proximity profile

As the ramped profile is a critical condition for this bake process, I don't
want to spend too much time going into further detail, in case you don't have
ramped proximity capability.  If you would like additional discussion on this or
related topics, feel free to give me a call (I've pretty extensive experience
with thick film coating, even up to a 65 µm single coat of AZ9260, and single
coats in excess of 100 µm with other positive materials).

Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.

 -----Original Message-----
From:   [email protected] [mailto:[email protected]]  On
Behalf Of Eric Miller
Sent:   Thursday, July 08, 2004 3:08 PM
To:     'General MEMS discussion'
Subject:        [mems-talk] UV Cure of Thick Photoresist

Can anyone suggest a robust, thick resist (up to 20 um) UV/hot plate cure
process for AZ9260 or AZ4620 used as a mask in a DRIE Bosch process?  Our
standard process uses either a hot plat or oven, and we would like to find a
process that would maintain better resist sidewall profiles, as well as
increase the selectivity of the mask to silicon.  We are planning to run
some tests using a Fusion M150-PC.


Eric Miller
[email protected]
Ph:  206 616-3855
www.watechcenter.org




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics