Does water attack the attachment of PDMS?
2004-08-11
X J
2004-08-13
Jayna Shah
Does water attack the attachment of PDMS?
Jayna Shah
2004-08-13
Jason,

Look at Whitesides publication for improving bond strength with PDMS.
http://gmwgroup.harvard.edu/domino/html/webpage/homepage2.nsf

As far as I know, plasma is supposed to improve the PDMS adhesion to glass
because it activates
the PDMS surface and makes it hydrophilic, but I am not too sure about SU-8.

Jayna



> ATTACHMENT part 3.9 message/rfc822
From: "X J"
To: [email protected]
Date: Wed, 11 Aug 2004 20:13:18 +0000
Subject: [mems-talk] Does water attack the attachment of PDMS?

Dear Colleagues,
I worked on the microfluidic devices. When I use plasma treat the PDMS
and SU-8 (on a glass slide) sample, and try to attach them. The attachment
seems very strong at the beginning. I can even break the PDMS without
getting PDMS detached from the SU-8 layer. But when I inject the water or
put the device into the water for about 24 hours, which is typically my
experiment period, the PDMS and SU-8 are detached from each other. Does
that mean the water is able to attack the bonding between PDMS and SU-8? Do
you have any suggestion on how to improve the bonding?
Thanks a lot!


Sincerely,
Jason



---------------------------------
Do you Yahoo!?
Yahoo! Mail is new and improved - Check it out!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.