Dear all:

I'm trying to make schottky contact on n-type Si by evaporating thin Pt
layer followed by thick Au layer and then liftoff.  The metal patens will be
on both Si (active region) and oxide (isolation region).  However, I found
the adhesion between Pt and Si is ok but it's relatively poor between Pt and
oxide. Does anyone has any suggestion on enhancing the adhesion without
introduce an extra layer between Pt and Si?  Any suggestion is highly
appreciate.

Hao-Chih Yuan
Research Assistant
Dep. of Electrical & Computer Engineering
University of Wisconsin - Madison
1415 Engineering Drive, 3557EH,
Madison, WI, 53706
TEL: (608)262-1648
email: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer