MEMSnet Home: MEMS-Talk: RIE of Aluminum
RIE of Aluminum
2004-10-26
Vivek Mukhatyar
2004-10-26
[email protected]
2004-10-26
Isaac Wing Tak Chan
2004-10-26
William Lanford-Crick
2004-10-27
Tripp, Marie Kathleen
Re: silicon nitrade membranes
2004-11-02
Romana Maryla Krolikowska
2004-10-27
HAN Anpan
2004-10-27
Michael D Martin
RIE of Aluminum
[email protected]
2004-10-26
Hi Vivek,

I have found that Al acts as an etch stop for SF6 RIE etch.
I guess that it should behave in a similar fashion for CHF3
gas in the RIE. You might want to try wet etching of Al
instead of RIE if that is permissible by your process.

Anupama

 Hey all,
>
> I have a pattern on an aluminium-Al2O3 wafer  (array of
> holes of 50 microns). I want to etch out the aluminum that
> has been exposed by the pattern.  The layer of aluminium
> on the aluminum oxide is about 700 microns.  Does anyone
> know what is the best photoresist that will last in the
> RIE and how long should I leave the chips in the RIE to
> etch out approximately 700 microns?   Also if anyone knows
> the chemistry that I should use in the RIE to efficiently
> etch the aluminum and not the Al2O3 would be very helpful.
>
> Thank you everyone in advance.  You guys have been great
> help.
>
> Vivek
> _______________________________________________
> [email protected] mailing list: to unsubscribe or
> change your list options, visit
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing
> services. Visit us at http://www.memsnet.org/

Anupama V. Govindarajan
PhD Student
EE MEMS laboratory
Department of Electrical Engineering
University of Washington
Campus Box 352500, Seattle WA 98195
Phone: (206)-221-5340
email: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.