MEMSnet Home: MEMS-Talk: Thick Photoresist with high transparency
Thick Photoresist with high transparency
2004-10-27
Carsten Dehoff
2004-10-27
Brubaker Chad
Thick Photoresist with high transparency
Carsten Dehoff
2004-10-27
Hi everybody,

does anyone know/have experience with a negative photo resist (and spin
parameters) for a 7-8 um thick PR film?
My problem is that the resist we are using right now is almost black so I
can hardly see my structures underneath the PR (when aligning).

Thanks!

Carsten

Aachen University


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of [email protected]
Sent: Wednesday, October 27, 2004 2:16 AM
To: [email protected]
Subject: MEMS-talk Digest, Vol 24, Issue 34

Send MEMS-talk mailing list submissions to
        [email protected]

To subscribe or unsubscribe via the World Wide Web, visit
        http://mail.mems-exchange.org/mailman/listinfo/mems-talk
or, via email, send a message with subject or body 'help' to
        [email protected]

You can reach the person managing the list at
        [email protected]

When replying, please edit your Subject line so it is more specific than
"Re: Contents of MEMS-talk digest..."


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics