MEMSnet Home: MEMS-Talk: RuO2 deposition
RuO2 deposition
2004-11-26
Philippe Combette
2004-11-27
[email protected]
RuO2 deposition
Philippe Combette
2004-11-26
Hi all,
I have some difficulties in RuO2 films deposition by sputtering on
different substrates like SiO2 and SiNx low stress. When the thickness is
more than 120 nm, the film peel off on SiNx. I tried different clean
methods (RCA, pirahna, with or without HF dip), but finally after few days,
the films peel off. Is anyone got the same difficulties ?
Thank you.
Philippe Combette


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group
Tanner EDA by Mentor Graphics