MEMSnet Home: MEMS-Talk: Bonding Kapton to glass
Bonding Kapton to glass
2005-01-25
Joseph P Valentino ([email protected])
2005-01-26
Joseph P. Valentino
2005-01-26
Shay Kaplan
2005-01-26
Bill Moffat
2005-01-26
Joseph P. Valentino
2005-01-26
Michael D Martin
2005-01-26
Brubaker Chad
2005-01-26
Joseph P. Valentino
2005-01-26
[email protected]
Bonding Kapton to glass
Joseph P. Valentino
2005-01-26
Shay and Chad, thanks for the suggestion - I have tried BCB and while
Kapton will stick, it is easily removed with a slight tug at the corner of
the film.  I'm looking for something that can withstand a little more force.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer