Surface properties of ITO
2005-02-03
Paolo Tassini
2005-02-03
Boris Kobrin
Surface properties of ITO
Boris Kobrin
2005-02-03
Hi Paolo,

If you will find that oxygen plasma (ozone/UV treatment) don't give you long
lasting surface modification, we can help you to deposit very thin (nm range
thickness) layers, which would perform much better. You may even engineer
exact wetting properties (contact angle), roughness and thickness you need.
Please contact me if you have any questions.

Regards,
Boris
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing