I was wondering does anyone have a good spin-bake recipe for obtaining 15um
thick layer of PMMA. I do 3-layer deposition-bake in order to obtain this
thickness, but after the second bake, the PMMA cracks. Any help would be greatly
appreciated.
Thank you,
Lidia