Hi,

A very complete overview about etch rates of different SiO2's is given
by Witvrouw et al., "A comparison between wet HF etching and vapor HF
etching for sacrificial oxide removal", SPIE. I don't know how old it is
though.

Best regards
Christian Spoerl