Hi,

depending on your HBC module, you can decrease the helium pressure in your
recipe. If that is not possible, you are still using an HBC1 module; in
this case the only possibility is to use a wafer to mount your sample on
(by glue or photoresist). You can also try decreasing the helium pressure
manually on the HBC module.

Marco

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.