MEMSnet Home: MEMS-Talk: Q: PDMS mechanical property
Q: PDMS mechanical property
2005-05-03
CY Park
2005-05-03
Patrick Roman
2005-05-04
emelianov
Q: PDMS mechanical property
Patrick Roman
2005-05-03
Chan-

This is a good paper for the answers to your questions.  Armani et al,
"Re-configurable Fluid Circuits by PDMS Elastomer Micromachining", google
will find it for you.

--
Patrick Roman, M.S.


-----Original Message-----
From: CY Park
Subject: [mems-talk] Q: PDMS mechanical property

Does anybody know about the mechanical properties (such as Young's modulus,
Poisson Ratio, density, etc) of PDMS?
I am using Sylgard 184 (Dow chemical).
If possible, I want to know the properties of PDMS of each mixing ratio
(such as 5:1, 10:1, 20:1).
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.