Hasan-

I have 2 data points for PDMS tan Delta:

Tan Delta = 0.03 below 100Hz, increasing to 0.2 at 10kHz

Reference:  Viscoelastic Solids, Roderic S. Lakes, CRC Press, New York, 1999

Not the value you are looking for, but maybe helpful.

Tan Delta data can be quite hard to find for this material, good luck.

Patrick Roman, M.S.
Microsystems Engineer

-----Original Message-----
From: [email protected]
Subject: [mems-talk] PDMS loss tangent at very high frequency

I was wondering if anybody knows the loss tangent of PDMS at very high
frequency, 10GHz.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing