About Negative Photoresist
2005-05-08
[email protected]
2005-05-09
Kristjan Leosson
2005-05-09
Brubaker Chad
2005-05-09
Brubaker Chad
2005-05-11
[email protected]
About Negative Photoresist
Kristjan Leosson
2005-05-09
You can use maN-490 from www.microresist.de for film thickness in the
range 5-16um. Since it is a negative resist, you can use flood exposure on
the final pattern and remove it with your standard developer.  You can
also use organic solvents.

Kristjan Leosson, Ph.D.
Process Development Engineer
Lumiscence A/S

-----Original Message-----
From: [email protected]
Subject: [mems-talk] About Negative Photoresist

I'm looking for negative photo resist for 5 to 30 um processing. In this
process the resolution is not important. The resist and developer should (if
possible) be nontoxic. It would nice to have resist stripped in Ace or in
some AZ developer. I know Japanese have resist called NFR015, but they
doesn't seem to sell it to Europeans. I wonder what you might know about
PR's or PR vendors?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Nano-Master, Inc.