2005-05-20
Hello,

We're interested in encapsulating some electrolyte-insulator-silicon (EIS)
sensors in glass microfluidics.  My question is whether anodic bonding of
the pyrex will cause damage to the implant traces required in the sensor
design.  I suppose the temperatures are too low to cause damage, but will
the large electric field or ion migration be a problem?  It should be
pointed out that the implants will be covered by 800 nm of nitride, so
direct bonding of the pyrex will be to the nitride.  But there will some
windows in the nitride where the underlying silicon will be exposed to an
air gap (fluidic channel ~ 3 microns) between the pyrex and the surface.
Any insight or references would be greatly appreciated.

Thanks ahead of time,

Mike


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing