I have some parts made from an Aluminum Titanium Carbide substrate. The
parts have slots cut into them 6 mils wide 2 mils deep. We need to coat
the parts with a 2 micron film of AZ-4620 or AZ-4902. It appears to pull
back from the sharp edges of the slots in some cases. Has anyone any
thoughts on substrate wetting an pull back with these materials

Regards,

Steve Adamson
Market Manager - Hard Disk Drives
Asymtek
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing