hello listers,
   i am a student at SIU carbondale. i am try to fabricate a
free standing thin film by first coating a NaCl crystal and then
dissolving a portion of it in water to obtain the freestanding
sample. however, since the film also needs to be suspended on a
silicon frame, i am getting a discontinuous film due to the
boundary between the NaCl crystal and the silicon frame glued to
it. could you suggest a more feasible/suitable option to obtain
a freestanding flim? i am not very comfortable with masking and
etching, although i am aware that such procedures have been
utilised in achieving the results i desire.
   any and all suggestions would be very welcome.
thankyou very much and have a nice day,
regards,
sailesh.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics