MEMSnet Home: MEMS-Talk: Low refractive index optical polymer
Low refractive index optical polymer
2005-06-23
Harald Walter
Low refractive index optical polymer
Harald Walter
2005-06-23
Dear Kristjan,

Goodfellow offers FEP with a index of 1.344
http://www.goodfellow.com/csp/active/STATIC/E/Fluorinated_Ethylene_Propylene_Cop
olymer.HTML
Applications include coatings and protective linings,
chemical and medical equipment, extruded insulation
and glazing film for solar panels. Maybe it can be
spin-coated.

Harald


> Can someone recommend a commercially available
optical
> polymer with refractive index around 1.38 (in the
visible)
> for spin-coating.
>
> Thanks
>
> Kristjan Leosson
> Lumiscence A/S
>






___________________________________________________________
Gesendet von Yahoo! Mail - Jetzt mit 1GB Speicher kostenlos - Hier anmelden:
http://mail.yahoo.de
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics