Hi all,

By accident, a colleague of mine had his plating mask (of patterned
SU-8) peeled off by his electroplating solution which was heated at 60C.
The 30um SU-8 was spun onto a copper seed on top of a silicon substrate
and would come off midway during the plating process. Using omnicoat has
to an extent helped to prevent this.

Anyway Id like to create a similar freestanding 'layer' of SU-8 to
hopefully do some screen printing but was hoping someone could suggest
me a simpler route than the one above. Thanks very much.

I Samad
Cambridge University Engineering Dept
+44 1223 764 205


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.
Nano-Master, Inc.