MEMSnet Home: MEMS-Talk: S1813: time and temperature hardbake before SiDRIE
S1813: time and temperature hardbake before SiDRIE
2005-07-25
Jobert van Eisden
S1813: time and temperature hardbake before SiDRIE
Jobert van Eisden
2005-07-25
Yes, I have nothing but resist faceting going on during dry etching,
which causes sloped sidewalls even if you start out with nice and
vertical, and this is in no means beneficial for the resulting etch
profile. Maybe if you have incredible selectivity it will work.

Jobert van Eisden
SUNY Albany

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Harrick Plasma, Inc.