  I am looking for information on bonding or sealing of glass to glass. The
bond should be direct--I would like to avoid using bonding films or
adhesives.  The bonding can be done at any temperature provided the glass
parts are not deformed or distorted. I would appreciate any information or
leads.

Thanks,

Tang Yanghua

MEMS LAB, Tsinghua Univ.
P.R.China
100084

86-10-62785565
FAX: 86-10-62784691


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review