A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: PDMS binding to glass
Re: PDMS binding to glass
2005-11-21
Martijn van Duijn
Re: PDMS binding to glass
Martijn van Duijn
2005-11-21
I have had modest success with precoating glass with a monolayer of a
silane, such a vinyl silane. The vinyl group should get meshed up in the
PDMS polymer network, the silane bonds to the glass. I haven't tested it
exhaustively, but you may look into that direction to see if it is good
enough for you. Gelest sells a big selection of silanes.

Martijn

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing