Dear Dr. Ramaraju,

I don't know of anyone manufacturing 2" SOI wafers. I actually don't believe 3"
is commercially available either, but I am not completely sure.

I work for a company called BCO Technologies. We are a manufacturer of 100, 125
and 150 mm diameter SOI wafers, with silicon device layers of 2 um and above.
The thickness uniformity we can achieve is
+/-0.5 um, so the 10% you need on a 20um layer is not a problem.

If you think you can somehow use 100 mm (that is, about 4"...) wafers, please
let me know, and I would be happy to send you a quotation.

Best regards,

Karin

********************************************************************************
***
Dr. Karin Hermansson
European Marketing Manager
BCO Technologies PLC
339 Glen Road
Belfast BT11 8BU
United Kingdom
Tel: +44 1232 615599
Fax: +44 1232 616788
Mob: +44 410 423479
**** Don't forget - we're on the Internet! http://www.bco-technologies.com ****
********************************************************************************
***

-----Original Message-----
From:    PC :[email protected] [SMTP:PC :[email protected]]
Sent:   Tuesday, June 09, 1998 7:57 AM
To:      [email protected];  [email protected];  Karin.Hermansson
@BCO-Technologies.com
Subject:        2 inch wafers



I am looking for 2 inch dia <100>  n-type bonded wafer with sandwitched
1um
Si O2 layer.  The wafer may be Si <100>  base with thickness >250um,
SiO2 layer with
1Um +/- 10% thickness and then n-type  Si layer <100> with 20um +/- 10%
thickness.

Does anyone know who sells them and at what price?

TThanks in advance


 Dr. GV Ramaraju
 Department Of  Electronics
 New Delhi, India



 << File: ENVELOPE.TXT >>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group