Dear MEMS community,
Is TMAH compatible with a 1 micron, 2-metal process
CMOS ASIC foundry? Can TMAH be used for wet etching?
Are there any contamination and corrosion issues? If
so, what are the safety/set up requirements? Is there
any other CMOS compatible etchant for Si bulk
anisotropic wet etching? Awaiting your valuable
inputs.

thanks,
Srikoundinya Punnamaraju
SITAR
India.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics