Deposition of nitride on metal
2006-02-05
Rakesh Poddar
2006-02-05
PRAMOD GUPTA
Deposition of nitride on metal
Rakesh Poddar
2006-02-05
Hi,

  I want to electrically insulate my metal patterns (Al, Cr) by depositing a
nitride layer...Is it possible to deposit LPCVD or PECVD nitride on the metal
layer particuarly Al and Cr.. If anybody has prior experience on this kind of
process, please comment...

  Thank you
  Rakesh