Hi, I'm a year 12 student in Australia.  I have to do a project on
silver electroplating.  I have great difficulties to find information in
this topic.  I just wonder if you have any information on this subject that
you can kindly sent it to me.  I will be very grateful.

                                                from
                                                       Bonnie